LANL Mo Target Process
for Sr-82*
•
Dissolve target in 30% H
2
O
2
•
Pass solution through cation exchange column
•
Wash with 10% H
2
O
2
•
Elute column 6 M HCl
•
Convert to 0.1 M HCl
•
Load onto new cation column
•
Wash column with 0.5 M H
2
SO
4
•
Elute Sr-82 with 1 M
HCl